Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.76 - 3.40 GPa | 255 - 493 ksi | Average value: 2.41 GPa Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 0.800 - 3.40 GPa @Temperature 60.0 - 120 °C |
116 - 493 ksi @Temperature 140 - 248 °F |
Average value: 2.45 GPa Grade Count:4 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |