Material Notes:
AntistaticHomopolymerNarrow molecular wt. dist.NucleatedApplications: CapsClosuresConsumer applications
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength, Yield 39.3 MPa
5700 psi
ASTM D638
Elongation at Yield 8.5 %
8.5 %
ASTM D638
Flexural Modulus 1.76 GPa
255 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
73°F; ASTM D256
Descriptive Properties Value Comments
Characteristics Antistatic, Nucleating agent
Forms Pellets
Processing Methods Injection molding
Users viewing this material also viewed the following: