Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem FT200WV Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem FT200WV Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Good mold release, nucleated, excellent rigidity and hardness.Applications: Suggested uses include housewares, caps and closures, fast-cycle injection molding.Process: Injection Molding.This resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.1520 issued by the Food and Drug Administration. The additives present are covered in appropriate regulation by FDA.Information provided by Braskem
Physical Properties Metric English Comments
Melt Flow 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength 38.6 MPa
5600 psi
2 in/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
2 in/min; ASTM D638
Flexural Modulus 1.76 GPa
255 ksi
0.05 in/min, 1% secant; ASTM D-790A
Izod Impact, Notched 0.374 J/cm
0.700 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648B
Copyright © lookpolymers.com All Rights Reserved