Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Ravago Manufacturing Americas, LLC
Trade Name Hylon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ravago Manufacturing Americas Hylon® N1200STHL BK Nylon 6/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in North America Additive: Heat Stabilizer and Lubricant Features: Lubricated, Good Toughness and Heat StabilizedRoHS CompliantForm: Pellets Color: BlackInformation provided by Ravago.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Density 1.08 g/cc
0.0390 lb/in³
ISO 1183
Water Absorption 1.2 %

@Time 86400 sec
1.2 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.017 - 0.021 cm/cm
0.017 - 0.021 in/in
ASTM D955 and ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 51.7 MPa
7500 psi
ASTM D638
52.0 MPa
7540 psi
ISO 527-2
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
68.9 MPa
10000 psi
ISO 178
Flexural Modulus 1.55 GPa
225 ksi
ISO 178
1.76 GPa
255 ksi
ASTM D790
Izod Impact, Notched 8.54 J/cm
16.0 ft-lb/in
ASTM D256
Izod Impact, Notched (ISO) 861 kJ/m²
410 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
420 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C
135 °F
Unannealed; ASTM D648