Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.80 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.76 - 2.80 GPa
255 - 406 ksi
Average value: 2.26 GPa Grade Count:56
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Flexural Modulus 1.90 - 2.80 GPa

@Temperature -40.0 - 71.0 °C
276 - 406 ksi

@Temperature -40.0 - 160 °F
Average value: 2.35 GPa Grade Count:1
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Flexural Modulus 2.40 - 2.80 GPa
348 - 406 ksi
ASTM D790
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Flexural Modulus 2.60 - 2.80 GPa
377 - 406 ksi
ASTM D790
Loxim 500 00V0 Polycarbonate/Acrylonitrile Butadiene Styrene
Information provided by Loxim Industries
Flexural Modulus 2.60 - 2.80 GPa
377 - 406 ksi
ASTM D790
Loxim 841 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 0.690 - 2.80 GPa
100 - 406 ksi
Average value: 2.22 GPa Grade Count:10
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..