Polymer Property : Flexural Modulus = 1.32 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.32 GPa
192 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 30-3000
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 1.32 GPa
192 ksi
1% Secant; ASTM D790
LyondellBasell Alathon® M6080WC High Density Polyethylene
ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c..
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
Hyosung Topilene B240T PP
B240T Extrusion Impact CopolymerApplications:Thermoforming sheetStationary sheetCharacteristics:High impactHigh stiffnessInformation provided by Hyosung Corporation
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
Hyosung Topilene J440F PP
J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Flexural Modulus 1.32 GPa

@Thickness 6.40 mm
192 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance
Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid..
Flexural Modulus 1.32 GPa

@Thickness 6.40 mm
192 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Flexural Modulus 1.32 GPa
191 ksi
ASTM D790
Iran Petrochemical (PCC) 52511 High Density Polyethylene
52511 is a HDPE copolymer injection molding grade for applications requiring a good balance between physical properties and flowability, like housewares and toys.Application: houseware, injection m..
Flexural Modulus 1.32 GPa
191 ksi
ASTM D790B
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Flexural Modulus 1.32 GPa
191 ksi
ASTM D790B
Lotte Chemical Titan TITANPRO® SM840 Polypropylene impact copolymer
Titanpro® SM840 is an extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant..
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H6007JU High Density Polyethylene Injection Molding
Key Characteristics:Good processabilityHigh rigidityHigh impact resistanceGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drink, bottles, pallet, garbage bins, con..
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P400S Polypropylene Flat Yarn/Sheet
Key Characteristics:High outputGood mechanical propertiesRecommended Applications:Stretched tapeMonofilament for woven bag, woven sheet, rope, strap and sheetInformation provided by SCG Chemicals
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding
Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys..
Flexural Modulus 1.32 GPa
192 ksi
Zylog Hipolyene® 1046 IFL Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.32 GPa
192 ksi
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.32 GPa
192 ksi
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.32 GPa
192 ksi
Zylog Hipolyene® 8110 HF Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.32 GPa
191 ksi
Tangent Method 1; ASTM D-790
Bapolene® 3262 Polyethylene, Injection Grade
Narrow molecular weight distribution injection molding resin. This resin offers intermediate flow, excellent ESCR, excellent impact and good warp resistance. This product meets FDA standards for f..
Flexural Modulus 1.32 GPa
191 ksi
Secant @ 1% strain; ASTM D-790
Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade
Polypropylene extrusion impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA regulation 21 CFR ..
Flexural Modulus 1.32 GPa
191 ksi
ASTM Test
BASF Ultraform N 2640 Z6 UNC POM
Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength.
Flexural Modulus 1.32 GPa
192 ksi
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.