Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.32 GPa | 192 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 30-3000 Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | 1% Secant; ASTM D790 |
LyondellBasell Alathon® M6080WC High Density Polyethylene ApplicationsALATHON M 6080WC is a natural, high density, polyethylene homopolymer resin with a narrow molecular weight distribution formulated for use as primary insulation for coaxial and control c.. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | ASTM D790 |
Hyosung Topilene B240T PP B240T Extrusion Impact CopolymerApplications:Thermoforming sheetStationary sheetCharacteristics:High impactHigh stiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | ASTM D790 |
Hyosung Topilene J440F PP J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.32 GPa @Thickness 6.40 mm |
192 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Flexural Modulus | 1.32 GPa @Thickness 6.40 mm |
192 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H6007JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh rigidityHigh impact resistanceGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drink, bottles, pallet, garbage bins, con.. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P400S Polypropylene Flat Yarn/Sheet Key Characteristics:High outputGood mechanical propertiesRecommended Applications:Stretched tapeMonofilament for woven bag, woven sheet, rope, strap and sheetInformation provided by SCG Chemicals |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P403J Polypropylene Injection Molding Key Characteristics:High stiffnessHigh glossGood processabilityOdorlessSafe for food contactRecommended Applications:General purpose housewaresFood containersMedical instrumentsInfant articles, toys.. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | |
Zylog Hipolyene® 1046 IFL Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | |
Zylog Hipolyene® 1048 X1 Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | |
Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | |
Zylog Hipolyene® 8110 HF Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Flexural Modulus | 1.32 GPa | 192 ksi | |
Zylog Hipolyene® 8110 EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |