Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® 3262 Polyethylene, Injection Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Bapolene®
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 3262 Polyethylene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Narrow molecular weight distribution injection molding resin. This resin offers intermediate flow, excellent ESCR, excellent impact and good warp resistance. This product meets FDA standards for food contact applications.Applications: General purpose injection molding, caps, closures, pails.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 190 °C
12 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 480 %
480 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.32 GPa
191 ksi
Tangent Method 1; ASTM D-790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Descriptive Properties Value Comments
Process Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: