Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hyosung Topilene J440F PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene J440F PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.4 MPa
4410 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 1.32 GPa
192 ksi
ASTM D790
Izod Impact, Unnotched 0.785 J/cm
1.47 ft-lb/in
ASTM D256
0.343 J/cm

@Temperature -10.0 °C
0.643 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 161 °C
322 °F
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved