Material Notes:
Grade H03G-05 is a polypropylene homopolymer designed for BOPP applications and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Food PackagingOverwrapMetallized FilmBenefits:BarefootGood Optical PropertiesConsistent ProcessingHigh Speed ProcessingHigh Strength PropertiesInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 3.4 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.4 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.2 MPa
4670 psi
ASTM D638
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ASTM D648
Descriptive Properties Value Comments
Process Film
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved