PolyMirae Moplen RP344R Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen RP344R Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for injection molding of houseware, thin walled articles for food and non food applications, caps and lids Moplen RP344R meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520 for food contact.Features: Excellent Transparency; High gloss; Good Color; Good mechanical property balanceApplications: Houseware; TWIM; Caps and lidsInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 24 g/10 min

@Load 2.16 kg,
Temperature 230 °C
24 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 29.4 MPa
4270 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
Izod Impact, Notched 0.196 J/cm

@Temperature -20.0 °C
0.367 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.490 J/cm

@Temperature 23.0 °C
0.918 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Optical Properties Metric English Comments
Haze 16 %
16 %