Material Notes:
Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection molding of pallet. Moplen EP300K meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010.Features: Very high impact even at low temperature combined with a good stiffness/Optimized balance of stiffness and toughness/Low warpageApplications: E&E/Houseware/CratesInformation provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Temperature -20.0 °C
0.918 ft-lb/in

@Temperature -4.00 °F
0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525