Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.38 - 2.41 GPa | 200 - 350 ksi | ASTM D790 |
Alcoa KAMA 3300 Very High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Flexural Modulus | 1.73 - 2.41 GPa | 251 - 350 ksi | ASTM D790 |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Flexural Modulus | 2.07 - 2.41 GPa | 300 - 350 ksi | ASTM D790 |
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail en.. |
|||
Flexural Modulus | 1.93 - 2.41 GPa | 280 - 350 ksi | Average value: 2.18 GPa Grade Count:25 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Flexural Modulus | 0.827 - 2.41 GPa | 120 - 350 ksi | Average value: 1.24 GPa Grade Count:88 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
Flexural Modulus | 1.52 - 2.41 GPa | 220 - 350 ksi | Average value: 2.10 GPa Grade Count:10 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |