Dow HDPE 12450N High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Impact Grade
Manufacturer Dow Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow HDPE 12450N High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DOW HDPE 12450N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness with moderate stiffness. This resin has good processability over a wide range of molding conditions. Typical applications are structural foam, tote boxes, and industrial containers. It complies with FDA regulation 21 CFR 177.1520 (c) 3.2(a) for food contact applications.Data provided by Dow Chemical.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
Viscosity 75000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
75000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
160000 cP

@Shear Rate 1000 1/s,
Temperature 190 °C
160000 cP

@Shear Rate 1000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
250000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
250000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Melt Flow 12 g/10 min

@Load 2.16 kg
12 g/10 min

@Load 4.76 lb
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.6 MPa
2700 psi
Tensile Strength, Yield 18.6 MPa
2700 psi
Elongation at Break 650 %
650 %
Modulus of Elasticity 0.559 GPa
81.1 ksi
Molded Sample 2% Secant Modulus
Flexural Modulus 0.827 GPa
120 ksi
Izod Impact Resistance 7.47 J/cm²
35.6 ft-lb/in²
Thermal Properties Metric English Comments
Vicat Softening Point 123 °C
253 °F