Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 350 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.38 - 2.41 GPa
200 - 350 ksi
ASTM D790
Alcoa KAMA 3300 Very High Impact Polystyrene  (discontinued **)
CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat..
Flexural Modulus 1.73 - 2.41 GPa
251 - 350 ksi
ASTM D790
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..
Flexural Modulus 2.07 - 2.41 GPa
300 - 350 ksi
ASTM D790
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Primarily used for consumer packaging, VersaTech RPET delivers on excellent clarity and high gloss, while providing good impact and tear resistance properties that are demanded in today’s retail en..
Flexural Modulus 1.93 - 2.41 GPa
280 - 350 ksi
Average value: 2.18 GPa Grade Count:25
Overview of materials for Acrylic/Polycarbonate Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap..
Flexural Modulus 0.827 - 2.41 GPa
120 - 350 ksi
Average value: 1.24 GPa Grade Count:88
Overview of materials for Cellulose Acetate Butyrate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value..
Flexural Modulus 1.52 - 2.41 GPa
220 - 350 ksi
Average value: 2.10 GPa Grade Count:10
Overview of materials for ABS/PVC Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW..
Copyright © lookpolymers.com All Rights Reserved