Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Impact Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionLP 552-01 is a U.L. approved narrow molecular weight copolymer high-density polyethylene combining good flow with excellent stiffness and cold temperature impact strength. It has good toughness and stress crack resistance.ApplicationApplications of LP 552-01 include food storage containers, housewares, toys, overcaps, and closures. This resin meets FDA Regulation CFR 177.1520 (c) 3.1.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.953 g/cc
0.953 g/cc
ASTM D792
ESCR 100% Igepal® 1.0 hour
1.0 hour
Condition B; ASTM D1693
Melt Index of Compound 20 g/10 min
20 g/10 min
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
1% secant; ASTM D790
Falling Dart Impact 176 J

@Temperature -40.0 °C
130 ft-lb

@Temperature -40.0 °F
F50; ASTM D3056
Users viewing this material also viewed the following: