Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & garden products and appliances. It is characterized by its easy mold flow, excellent physical property balance of stiffness and impact at room temperature and sub ambient conditions as well as finished product dimensional stability. Formolene® 2620A complies with the U. S. Food and Drug Administration regulation 21 CFR 177.1520(c)(3.4). This material may only be used in contact with foods of type I, II, III, IV-B, VI, VII, VIII and IX as described in Table 1 of 21 CFR 176.170(c)Specimens were injection molded according to the conditions specified in ASTM D4101Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Temperature 230 °C
20 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D785
Tensile Strength, Yield 17.9 MPa
2600 psi
2" (50mm) per min; ASTM D638
Elongation at Yield 5.0 %
5.0 %
2" (50mm) per min; ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 0.854 J/cm

@Temperature -30.0 °C
1.60 ft-lb/in

@Temperature -22.0 °F
ASTM D256
0.961 J/cm

@Temperature -18.0 °C
1.80 ft-lb/in

@Temperature -0.400 °F
ASTM D256
1.07 J/cm

@Temperature 0.000 °C
2.00 ft-lb/in

@Temperature 32.0 °F
ASTM D256
5.87 J/cm

@Temperature 23.0 °C
11.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Users viewing this material also viewed the following: