Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR MF5210-0301 DK GRAY 2451 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR MF5210-0301 DK GRAY 2451 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.010 - 0.020 cm/cm
0.010 - 0.020 in/in
ASTM D955
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 200 %
200 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 26.2 MPa
3800 psi
ASTM D790
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.29 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94
Descriptive Properties Value Comments
Features Flame Retardant
Medium Impact Resistance
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America