Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ISO 527 |
Polikim High Density Polyethylene (HDPE) High density polyethylene is preferred when resistance to chemicals and weather is the priority. As it can be supplied in large dimensions and can be welded, its use in construction of tanks and was.. |
|||
Tensile Strength, Ultimate | 19.6 - 49.0 MPa | 2840 - 7110 psi | Average value: 39.8 MPa Grade Count:29 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D638 |
Global J-1600 High Density Polyethylene Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D638 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC EF321 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties. Good Optical Properties. Additives : No Additive Applications: Agricultural FilmCSA No. 25895-47-0Information provided by LG Chemical |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | 500mm/min; ASTM D638 |
LG Chemical SEETEC EF443 Ethylene Vinyl Acetate Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural FilmCSA No. 24937-78-8Information provided by LG Chemical |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | |
Shinil Chemical SHINNANO PP Polymer Nanocomposite Bumper SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Tensile Strength, Ultimate | >= 19.6 MPa @Temperature 100 °C |
>= 2840 psi @Temperature 212 °F |
|
Sibur SKI-3 1st Grade, 2nd Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment. |
|||
Tensile Strength, Ultimate | >= 19.6 MPa @Temperature 100 °C |
>= 2840 psi @Temperature 212 °F |
|
Sibur SKI-3 1st Grade, 3rd Group Isoprene Rubber (IR) Nipol-IR 2200, Natsyn-2200, Kraton-IR 401. For production of tires and rubber technical articles of wide assortment. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D412 |
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D412 |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | 500 mm/min; ASTM D 412 |
Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.Ro.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D412 |
Lubrizol Estane® CR180A Thermoplastic Polyurethane Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | Cured 7 min at 177°C and Post Cured 16 hr at 232°C |
DuPont Performance Polymers VTR 8525 (GBLT-S) Peroxide Cured Fluoroelastomer (FKM) Formulation
(discontinued FormulationVTR-8525 |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | Cured 7 min at 177°C and Post Cured 2 hr at 232°C |
DuPont Performance Polymers VTR 8655 (GBL-S) Peroxide Cured Fluoroelastomer (FKM)
(discontinued **) FormulationVTR 8655 |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D412 |
SK Chemicals SKYTHANE® 400 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Ultimate | 19.6 MPa | 2840 psi | ASTM D412 |
SK Chemicals SKYTHANE® 370A T series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |