Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 28.91 - 49.0 MPa @Temperature 70.0 - 100 °C |
4193 - 7110 psi @Temperature 158 - 212 °F |
Average value: 43.3 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Tensile Strength, Ultimate | 28.91 - 49.0 MPa @Time 0.000 - 3.63e+6 sec |
4193 - 7110 psi @Time 0.000 - 1010 hour |
Average value: 43.3 MPa Grade Count:1 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Tensile Strength, Ultimate | 19.6 - 49.0 MPa | 2840 - 7110 psi | Average value: 39.8 MPa Grade Count:29 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Tensile Strength, Ultimate | 23.0 - 49.0 MPa | 3340 - 7110 psi | Average value: 38.2 MPa Grade Count:25 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |