Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Vulcanizate Elastomer (TPV)
Manufacturer Zylog Plastalloys
Trade Name Neoplast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Neoplast® 240 FT EB Thermoplastic Vulcanizate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Neoplast 240 FT EB is a hard, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding, Blow Molding and Extrusion applications.RoHS Compliant, UV StabilizedInformation provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
ASTM D 2240
44

@Treatment Temp. 150 °C,
Time 605000 sec
44

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 2240/ASTM D573
Tensile Strength, Ultimate 19.6 MPa
2840 psi
500 mm/min; ASTM D 412
21.6 MPa

@Treatment Temp. 150 °C,
Time 605000 sec
3130 psi

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
Elongation at Break 650 %
650 %
500 mm/min; ASTM D 412
553 %

@Treatment Temp. 150 °C,
Time 605000 sec
553 %

@Treatment Temp. 302 °F,
Time 168 hour
Heat Aging; ASTM D 412/ASTM D 573
100% Modulus 0.0118 GPa
1.71 ksi
500 mm/min; ASTM D 412
Tear Strength 63.7 kN/m
364 pli
500 mm/min; ASTM D 624
Compression Set 55 %

@Temperature 70.0 °C,
Time 79200 sec
55 %

@Temperature 158 °F,
Time 22.0 hour
ASTM B 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 140 °C
284 °F
Continuous; SAE J 2236
Brittleness Temperature -50.0 °C
-58.0 °F
ASTM D 746