Polikim High Density Polyethylene (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Polikim Polimer ve Kimya Sanay
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polikim High Density Polyethylene (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High density polyethylene is preferred when resistance to chemicals and weather is the priority. As it can be supplied in large dimensions and can be welded, its use in construction of tanks and waste water purification applications is ideal. It must not be treated equal to Ulpolen® group of products. There are some principal differences between the two types among which wear resistance is the major one. Wear resistance of high density polyethylene is distinctively lower.Information provided by Polikim Polimer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 1183
Water Absorption at Saturation 0.00 %
0.00 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Ultimate 19.6 MPa
2840 psi
ISO 527
Charpy Impact Unnotched NB
NB
ISO 179
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C
83.3 µin/in-°F
ISO 11359
Maximum Service Temperature, Air 70.0 °C
158 °F
continuous
Minimum Service Temperature, Air -25.0 °C
-13.0 °F