Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 45.0 MPa @Temperature 200 °C |
6530 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Compressive Strength | 45.0 MPa @Temperature 250 °C |
6530 psi @Temperature 482 °F |
ISO 604 |
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 1000 °C |
6530 - 7980 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 127 S Dense Refractory Castable Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 140 K Dense Refractory Silicon Carbide Castable This castable is based on silicon carbide and widely applied as the protective lining for pipes in boilers and incinerators. Curon 140 K has a high thermal conductivity and a good mechanical strengt.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 150 HS GM Dense Refractory Castable Description: Curon 150 HS GM is an abrasion resistant gunning castable for use up to 1500°C.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 C Dense Refractory Castable Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shoc.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 1400 °C |
6530 - 7980 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 1600 °C |
6530 - 7980 psi @Temperature 2910 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 TF Dense Refractory Castable Description: Curon 180 TF is a tabular alumina based castable, highly abrasion resistant, especially developed for application in the vacuum ladle treatment installation in the steel refinery.Remark.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast VIBRON 165 Dense Vibrating Refractory Castable Description: Vibron 165 is a low cement castable based on andalusite and especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provide.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 1000 °C |
6530 - 7980 psi @Temperature 1830 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 13 S Dense Refractory Castable Description: Curon 13 S is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/hol.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by .. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 C Dense Refractory Castable Description: A low carbon castable for use in reducing atmospheres. Curon 145 C has a coarse structure for improved thermal shock resistance.Remarks: These values apply to cast products.Information .. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 CC Dense Refractory Castable Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 1400 °C |
6530 - 7980 psi @Temperature 2550 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 160 HS Dense Refractory Castable Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shoc.. |
|||
Compressive Strength | 45.0 - 55.0 MPa @Temperature 100 °C |
6530 - 7980 psi @Temperature 212 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 180 T Sp Dense Refractory Castable Description: Curon 180 T special is a tabular alumina based castable, highly resistant against abrasion, dust erosion or heavy impact even at extremely high temperatures.Remarks: These values apply .. |
|||
Compressive Strength | 45.0 MPa @Temperature 200 °C |
6530 psi @Temperature 392 °F |
ISO 604 |
Victrex® PEEK 150FC30 Easy Flow Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy .. |