Material Notes:
Description: Because of the selection of raw materials, this castable has a high volume stability and a high strength up to high temperatures. In addition, Curon 160 HS has an excellent thermal shock resistance and abrasion resistance (7-10 cm3 according to ASTM C704-76a; in case of vibration cast 5-7cm3).Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.35 - 2.45 g/cc
0.0849 - 0.0885 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 45.0 - 55.0 MPa

@Temperature 1400 °C
6530 - 7980 psi

@Temperature 2550 °F
Cold Crushing Strength
65.0 - 75.0 MPa

@Temperature 100 °C
9430 - 10900 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.610 - 0.710 W/m-K

@Temperature 100 °C
4.23 - 4.93 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.800 - 0.900 W/m-K

@Temperature 1400 °C
5.55 - 6.25 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1400 °C
-0.400 - 0.400 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 62 %
62 %
CaO 5.0 %
5.0 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2350 kg
Mixing Water 8-10 liters
per 100 kgs dry material