Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast CURON 160 C Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 160 C Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 C has an excellent thermal shock resistance. It is largely used in the steel industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.50 - 2.60 g/cc
0.0903 - 0.0939 lb/in³
After drying at 110°C
Particle Size <= 10000 µm
<= 10000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 30.0 - 40.0 MPa

@Temperature 1600 °C
4350 - 5800 psi

@Temperature 2910 °F
Cold Crushing Strength
45.0 - 55.0 MPa

@Temperature 100 °C
6530 - 7980 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 - 0.870 W/m-K

@Temperature 100 °C
5.34 - 6.04 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.820 - 0.920 W/m-K

@Temperature 600 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.950 - 1.05 W/m-K

@Temperature 1600 °C
6.59 - 7.29 BTU-in/hr-ft²-°F

@Temperature 2910 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.550 - 0.550 %

@Temperature 1600 °C
-0.550 - 0.550 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 62 %
62 %
CaO 3.0 %
3.0 %
Fe2O3 1.0 %
1.0 %
SiO2 32 %
32 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2500 kg
Mixing Water 7-8 liters
per 100 kgs dry material