Polymer Property : Compressive Strength = 29.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CT-140S Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-170 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 24.5 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
3560 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-180G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HAPT-80S Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-160 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1500 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PT-170 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1500 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTA-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1500 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories PTF-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 350 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 662 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories SCX-90IP Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories SCX-90IP Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-150S High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-150 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-155 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 1350 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 19.6 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).