Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.002943 - 0.006867 GPa

@Temperature 110 °C,
Time 86400 sec
0.4269 - 0.9960 ksi

@Temperature 230 °F,
Time 24.0 hour
0.002943 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.4269 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.76768 W/m-K

@Temperature 260 °C
5.3191 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.82584 W/m-K

@Temperature 540 °C
5.7220 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.96542 W/m-K

@Temperature 800 °C
6.6892 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.0600 %

@Temperature 110 °C,
Time 86400 sec
-0.0600 %

@Temperature 230 °F,
Time 24.0 hour
1.0 %

@Temperature 1000 °C,
Time 10800 sec
1.0 %

@Temperature 1830 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 80 %
80 %
Descriptive Properties Value Comments
Installation Method Spray
Material Required for Estimating(kg/?) 2,350
Water Required for Casting(%) 13