Chosun Refractories HAPT-80S Plastic Refractory

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories HAPT-80S Plastic Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 9.62361e-7 - 0.00981 GPa

@Temperature 110 °C,
Time 86400 sec
0.000139581 - 1.42 ksi

@Temperature 230 °F,
Time 24.0 hour
0.014715 - 0.016677 GPa

@Temperature 1350 °C,
Time 10800 sec
2.1343 - 2.4188 ksi

@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength 19.6 - 29.4 MPa

@Temperature 110 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
49.0 - 58.8 MPa

@Temperature 1500 °C,
Time 10800 sec
7110 - 8530 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
58.8 - 68.6 MPa

@Temperature 1350 °C,
Time 10800 sec
8530 - 9960 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.3725 W/m-K

@Temperature 500 °C
9.5099 BTU-in/hr-ft²-°F

@Temperature 932 °F
1.5237 W/m-K

@Temperature 1000 °C
10.558 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.200 %

@Temperature 1350 °C,
Time 10800 sec
-0.200 %

@Temperature 2460 °F,
Time 3.00 hour
0.00 %

@Temperature 110 °C,
Time 86400 sec
0.00 %

@Temperature 230 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 82 %
82 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Main Applications Heat set Abrasion resistance High strength phosphate bond
Material Required for Estimating (kg/?) 2,900