Chosun Refractories SCX-90IP Plastic Refractory

Category Ceramic
Manufacturer Chosun Refractories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories SCX-90IP Plastic Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 8.66e-7 - 0.00589 GPa

@Temperature 350 °C,
Time 86400 sec
0.000126 - 0.854 ksi

@Temperature 662 °F,
Time 24.0 hour
9.62361e-7 - 0.006867 GPa

@Temperature 1000 °C,
Time 10800 sec
0.000139581 - 0.9960 ksi

@Temperature 1830 °F,
Time 3.00 hour
Compressive Strength 19.6 - 29.4 MPa

@Temperature 350 °C,
Time 86400 sec
2840 - 4270 psi

@Temperature 662 °F,
Time 24.0 hour
Cold Crushing Strength
19.6 - 29.4 MPa

@Temperature 1000 °C,
Time 10800 sec
2840 - 4270 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 6.65323 W/m-K

@Temperature 500 °C
46.0987 BTU-in/hr-ft²-°F

@Temperature 932 °F
7.80475 W/m-K

@Temperature 1000 °C
54.0774 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
limited
Shrinkage -0.160 %

@Temperature 350 °C,
Time 86400 sec
-0.160 %

@Temperature 662 °F,
Time 24.0 hour
-0.0500 %

@Temperature 1000 °C,
Time 10800 sec
-0.0500 %

@Temperature 1830 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
SiC 87 %
87 %
SiO2 4.0 %
4.0 %
Descriptive Properties Value Comments
Main Applications Resistance to chemical reaction High conductivity resistance to abrasion
Material Required for Estimating (kg/?) 2,400