Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 2840 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories CT-140 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 1000 °C,
Time 10800 sec
1420 - 2840 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CT-140 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 1350 °C,
Time 10800 sec
1420 - 2840 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories CT-140 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories HACT-165G High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 1350 °C,
Time 10800 sec
1420 - 2840 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-160 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 1500 °C,
Time 10800 sec
1420 - 2840 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories INCT-170 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories INCT-170 Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories MIX-1(1:4) Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTC-165 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
2130 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories PTF-180 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories CT-130 Fireclay Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 110 °C,
Time 86400 sec
1420 - 2840 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
Chosun Refractories TPA-175 Plastic Refractory
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 9.81 - 19.6 MPa

@Temperature 1000 °C,
Time 10800 sec
1420 - 2840 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-160 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Compressive Strength 14.7 - 19.6 MPa

@Temperature 1000 °C,
Time 10800 sec
2130 - 2840 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
Chosun Refractories HACT-165 High Alumina Castables
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved