Material Notes:
Special Properties: Non-wetting, Slag and Hot Abrasion ResistanceIndustry: SteelApplication: Trough LiningInformation provided by Sharadaa Ceramics Pvt. Ltd.
Physical Properties Metric English Comments
Bulk Density >= 2.65 g/cc
>= 0.0957 lb/in³
After Drying at 110°C
Grain Size <= 5000 µm
<= 5000 µm
Mechanical Properties Metric English Comments
Compressive Strength 29.4 MPa

@Temperature 110 °C
4270 psi

@Temperature 230 °F
Cold Crushing
53.9 MPa

@Temperature 1100 °C
7820 psi

@Temperature 2010 °F
Cold Crushing
78.5 MPa

@Temperature 1500 °C
11400 psi

@Temperature 2730 °F
Cold Crushing
14.7 MPa

@Time 86400 sec
2130 psi

@Time 24.0 hour
Cold Crushing
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1700 °C
3090 °F
Descriptive Properties Value Comments
Refractoriness >1820°C
Thermal Expansion 0.8
Reversible
Water Required to Mix 8-10%