Mechanical Properties Metric English Comments
Tensile Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Zytel® 444AHS is a toughened, heat stabilized, black polyamide 66 resin for injection molding. It is a high flow, processing friendly material.Information provided by DuPont Performance Polymers
Tensile Modulus 1.10 GPa

@Temperature 150 °C
160 ksi

@Temperature 302 °F
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame..
Tensile Modulus 1.10 GPa

@Temperature 120 °C
160 ksi

@Temperature 248 °F
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Modulus 1.10 GPa

@Temperature 90.0 °C
160 ksi

@Temperature 194 °F
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant
Polyamide 66 (PA66) based compound. High fluidity. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Blended with PA6.Availability: Africa & Middle East..
Tensile Modulus 1.10 GPa

@Temperature 60.0 °C
160 ksi

@Temperature 140 °F
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Modulus 1.10 GPa

@Temperature 90.0 °C
160 ksi

@Temperature 194 °F
LATI Latamid 6 S/30 PA 6, 30% Glass Bead Reinforced
Polyamide 6 (PA6) based compound. Glass beads. Very high dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indu..
Tensile Modulus 1.10 GPa

@Temperature 90.0 °C
160 ksi

@Temperature 194 °F
LATI Latamid 68 H2-V0 PA6/PA66 copolymer, Heat Stabilized, Flame Retardant
PA6/PA66 copolymer (PA6/PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Good surface appearance.Availability: Africa & Middle Ea..
Tensile Modulus 1.10 GPa

@Temperature 90.0 °C
160 ksi

@Temperature 194 °F
LATI Latan 23UV POM
Polyoxymethylene (POM). UV stabilized. Low viscosity. Very good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Tensile Modulus 1.10 GPa

@Temperature 60.0 °C
160 ksi

@Temperature 140 °F
LATI Latan 3E71 POM
Polyoxymethylene (POM). Toughened. High viscosity. Good elongation and impact resistanceAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by ..
Tensile Modulus 1.10 GPa

@Temperature 60.0 °C
160 ksi

@Temperature 140 °F
LATI Latene® 22H2 MX/25 PP Homopolymer, Heat Stabilized
Polypropylene homopolymer (PPh) based compound. Heat stabilized. Special mineral filler. Very good surface appearance.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A..
Tensile Modulus 1.10 GPa

@Temperature 60.0 °C
160 ksi

@Temperature 140 °F
LATI Latene® EP 7 TES/30 PP Copolymer, 30% Talc filled
Polypropylene copolymer (PPc) based compound. Aesthetic talc. Very good surface appearance. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfo..
Tensile Modulus 1.10 GPa

@Temperature 60.0 °C
160 ksi

@Temperature 140 °F
LATI Latigray 53/22-01 CX/25 PP Homopolymer, Impact Modified
Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformatio..
Tensile Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Zytel® FG408L NC010 is a general purpose, lubricated, impact modified polyamide 66 resin with superior toughness for injection molding applications. It has been developed for consideration into app..
Tensile Modulus 1.10 GPa

@Temperature 23.0 °C
160 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® LC6210 BK010 Nylon 612  (Unverified Data**)
Zytel® LC6210 BK010 is a highly toughened, heat stabilized polyamide 612 for extrusion, blow molding or processing by other techniques requiring high melt viscosity. It was previously coded Zytel®..