Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.58068 kN/m | 3.3125 pli | HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7002 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7811 Dot Matrix Printable Polyimide Label Material 3M™ Dot Matrix Printable Polyimide Label Material 7811 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand .. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7850TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7850 is a matte radiant white polyester label stock that offers . This label product utilizes 3M™ Adhesive 350 which is an universal adhesive for.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | to Stainless Steel, 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90°, 72 hr 158°F; ASTM D3330 |
3M 9456 Double Coated Tapes with Adhesive 340 3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These t.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7880 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Material 7880 is a 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for traditional.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7924 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | to Stainless Steel, 20 min dwell, 90° peel, 12"/min., 2 mil aluminum; ASTM D3330 |
3M 9462P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.58068 kN/m | 3.3125 pli | Stainless Steel, 90° peel, 2 mil aluminum foil backing, 15 min at RT, 4.9 mil; ASTM D3330 |
3M 9555 Adhesive Transfer Tapes with Adhesive 220 3M™ Adhesive Transfer Tapes with 3M™ Industrial Acrylic Adhesive 220 is an economical choice for general industrial bonding of metals, painted metals and high surface energy plastics.Information p.. |