3M 9456 Double Coated Tapes with Adhesive 340

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 9456 Double Coated Tapes with Adhesive 340.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Double Coated Tapes with 3M™ Adhesive 340 provide a combination of high initial adhesion and good shear holding power to a wide variety of materials, including many plastics and foams. These tapes are available with a thin polyester film or a tissue for dimensional stability and improved handling.Information provided by 3M
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Faceside Adhesive
50.8 microns
2.00 mil
Carrier
81.3 microns
3.20 mil
Backside Adhesive
109 microns
4.30 mil
Total Thickness
Mechanical Properties Metric English Comments
Peel Strength 0.3725 kN/m
2.125 pli
Stainless Steel, 90°, 15 min RT; ASTM D3330
0.4602 kN/m
2.625 pli
Polypropylene, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.5040 kN/m
2.875 pli
ABS, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330
0.526 kN/m
3.00 pli
Stainless Steel, 90°, 72 hr RT; ASTM D3330
0.58068 kN/m
3.3125 pli
Stainless Steel, 90°, 72 hr 158°F; ASTM D3330
1.0628 kN/m
6.0625 pli
Stainless Steel, 180°, 2 mil al foil, 72 hr RT; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 49.0 °C
120 °F
Long Term
66.0 °C
151 °F
Short Term
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Liner 55# Densified Kraft