Material Notes:
3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coatings, and slightly oily metals.Information provided by 3M
Physical Properties Metric English Comments
Thickness 27.9 microns
1.10 mil
Adhesive
66.0 microns
2.60 mil
Facestock
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.131 kN/m
0.750 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.153 kN/m
0.875 pli
HD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.1643 kN/m
0.9375 pli
LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.175 kN/m
1.00 pli
LD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.18626 kN/m
1.0625 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.1972 kN/m
1.125 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.20817 kN/m
1.1875 pli
Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.20817 kN/m
1.1875 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.219 kN/m
1.25 pli
Finely Textured Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.219 kN/m
1.25 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.23008 kN/m
1.3125 pli
Polycarbonate 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.25199 kN/m
1.4375 pli
HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.263 kN/m
1.50 pli
LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.263 kN/m
1.50 pli
LD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.27391 kN/m
1.5625 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.29582 kN/m
1.6875 pli
HD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
Polypropylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
HD Polyethylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.31773 kN/m
1.8125 pli
Polypropylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.3287 kN/m
1.875 pli
HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3287 kN/m
1.875 pli
Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.33964 kN/m
1.9375 pli
Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.351 kN/m
2.00 pli
LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.36156 kN/m
2.0625 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.3725 kN/m
2.125 pli
Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.3725 kN/m
2.125 pli
Polypropylene, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.38347 kN/m
2.1875 pli
Finely Textured Powder Coating, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.394 kN/m
2.25 pli
Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.4163 kN/m
2.375 pli
Finely Textured Powder Coating, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.42729 kN/m
2.4375 pli
Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.44921 kN/m
2.5625 pli
Polypropylene, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.47112 kN/m
2.6875 pli
Smooth Powder Coating, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.51494 kN/m
2.9375 pli
Polycarbonate 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.526 kN/m
3.00 pli
Smooth Powder Coating, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.570 kN/m
3.25 pli
Stainless Steel, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.570 kN/m
3.25 pli
Smooth Powder Coating, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.58068 kN/m
3.3125 pli
Smooth Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.5916 kN/m
3.375 pli
Polycarbonate 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.5916 kN/m
3.375 pli
Glass, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.60259 kN/m
3.4375 pli
Glass, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.60259 kN/m
3.4375 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.614 kN/m
3.50 pli
Glass, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.6355 kN/m
3.625 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.6355 kN/m
3.625 pli
Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.64642 kN/m
3.6875 pli
Glass, 90° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.657 kN/m
3.75 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.657 kN/m
3.75 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.657 kN/m
3.75 pli
Glass, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.66833 kN/m
3.8125 pli
Polycarbonate 180° Peel, Initial, 10 min dwell at RT; ASTM D3330
0.66833 kN/m
3.8125 pli
Smooth Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.69024 kN/m
3.9375 pli
Polycarbonate 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.69024 kN/m
3.9375 pli
Smooth Powder Coating, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.73407 kN/m
4.1875 pli
Glass, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.73407 kN/m
4.1875 pli
Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330
0.745 kN/m
4.25 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.75598 kN/m
4.3125 pli
Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.75598 kN/m
4.3125 pli
Smooth Powder Coating, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.789 kN/m
4.50 pli
Stainless Steel, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.79981 kN/m
4.5625 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
0.833 kN/m
4.75 pli
Glass, 180° Peel, Conditioned for 3 days at 70°C; ASTM D3330
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved