Material Notes:
3M™ Dot Matrix Printable Polyimide Label Material 7811 is a polyimide film product that offers ultra-high temperature performance. This label product utilizes 3M™ Adhesive 100, that can withstand up to 450°F (232°C) short-term heat resistance, has excellent solvent resistance, and exhibits low outgassing characteristics.Information provided by 3M
Physical Properties Metric English Comments
Thickness 25.4 microns
1.00 mil
Facestock, Matte White
50.8 microns
2.00 mil
Facestock, Polyimide Film
50.8 microns
2.00 mil
Adhesive
81.3 microns
3.20 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.351 kN/m
2.00 pli
Stainless Steel, 180° Peel, 10 min Dwell at RT; ASTM D3330
0.3725 kN/m
2.125 pli
Polycarbonate, 180° Peel, 10 min Dwell at RT; ASTM D3330
0.482 kN/m
2.75 pli
Epoxy PC Board, 180° Peel, 10 min Dwell at RT; ASTM D3330
0.482 kN/m
2.75 pli
Epoxy PC Board, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.58068 kN/m
3.3125 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.614 kN/m
3.50 pli
Polycarbonate, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.6355 kN/m
3.625 pli
Polycarbonate, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.6793 kN/m
3.875 pli
Epoxy PC Board, 180° Peel, Conditioned for 3 days at RT; ASTM D3330
0.6793 kN/m
3.875 pli
Polycarbonate, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.701 kN/m
4.00 pli
Stainless Steel, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
0.7231 kN/m
4.125 pli
Stainless Steel, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
0.73407 kN/m
4.1875 pli
Epoxy PC Board, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type 100 Acrylic
Liner 50# Densified Kraft