Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® GRM2600L ABS High Impact , good chemical resistance sheet grade ABS designed for refrigerator liner applications. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS Color Package may affect performance. Visual Fx PC+ABS in various metallic (Ares) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XP4034 ASA+PC Available in a wide range of colors. Recommended for unpainted exterior/high heat/high impact applications. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Geloy XTWM200 ASA (Europe-Africa-Middle East) ASA resin for injection molding. Excellent flow, colorability and outdoor weathering capability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Europe-Africa-Middle East) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.This .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | ASTM D790 |
Ineos Nova 3700 General Purpose Crystal Polystyrene
(discontinued **) Good balance of flow and strength, Good crack resistanceApplications: Single service wares, Blending resinExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the .. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 6.4 mm; ASTM D790 |
SABIC Innovative Plastics Lexan® FL2000 PC Lexan FL2000 is a medium flow specialty polycarbonate (PC) resin for structural foam molding, allowing for various weight reductions at 0.24"" (6.0mm) wall. This product offers low temperature impa.. |
|||
Flexural Yield Strength | 75.0 - 250 MPa | 10900 - 36300 psi | Average value: 141 MPa Grade Count:63 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 75.0 - 503 MPa | 10900 - 73000 psi | Average value: 266 MPa Grade Count:47 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
LG Chemical PI-642 ABS, Fitting, High Strength Information Provided by LG Chem |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Asia Pacific) RN0401 is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 20% PCR styrenic series resin content. Available in black only. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0401 PPE+PS (Europe-Africa-Middle East) Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS (Asia Pacific) LNP LUBRICOMP ZL003 is a compound based on PPE+PS Blend resin containing PTFE. Added features of this material include:internally Lubricated. Also known as LUBRICOMP ZL-4030 |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Europe-Africa-Middle East) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Europe-Africa-Middle East) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL GTX GTX954 PPE+PA (Europe-Africa-Middle East) NORYL GTX954 is an unfilled grade with improved processability and optimised heat/impact balance. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® XD1575S PBT+PC (Europe-Africa-Middle East) XENOY XD1575S is a high flow PC+PBT blend with good impact properties and good resistance to occasional solvent and gasoline contact. XENOY XD1575S has been specially developed for coated exterior b.. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL BN9003G PPE+HIPS PPE+PS blend. Unfilled. Blow molding. Excellent balance of impact and surface aesthetics. Suitable for automotive exterior components including spoilers. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PX1007 PPE+HIPS (Europe-Africa-Middle East) NORYL* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade, targeted for flat panel TV enclosures. It has a Vicat B/120 temperature of 96 degC and UL-94 V0 @ 1.5mm .. |
|||
Flexural Yield Strength | 75.0 MPa @Strain 3.50 % |
10900 psi @Strain 3.50 % |
2 mm/min; ISO 178 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Flexural Yield Strength | 75.0 - 85.0 MPa | 10900 - 12300 psi | ASTM D790 |
Chang Chun Plastic PBT1100L General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 75.0 MPa | 10900 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 315 PBT (Europe-Africa-Middle East) VALOX 315 is compliant with food contact regulations acc. to EC Reg. No. 10/2011. VALOX 315 can be applied for injection moulding and extrusion puposes. |