Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 22.1 - 44.8 MPa | 3200 - 6500 psi | Average value: 30.3 MPa Grade Count:11 |
Overview of materials for Ethylene Acrylic Acid This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 320 Cast Film Resin
(discontinued **) ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Westlake EP310 Low Density Polyethylene WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation .. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Dow INTEGRAL™ 906 Multilayer Adhesive Film INTEGRAL 906 Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethanes.Informa.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens,.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b.. |
|||
Film Tensile Strength at Break, TD | 22.1 MPa | 3200 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b.. |