Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners

Category Polymer , Film , Thermoset
Manufacturer Dow Chemical
Trade Name INTEGRAL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens, and Aluminum.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 280 %
280 %
ASTM D882
Film Elongation at Break, TD 490 %
490 %
ASTM D882
Secant Modulus, MD 0.131 GPa
19.0 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.138 GPa
20.0 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 12.2 g/micron
310 g/mil
ASTM D882
Elmendorf Tear Strength, TD 2.36 g/micron
60.0 g/mil
ASTM D882
Film Tensile Strength at Break, MD 25.5 MPa
3700 psi
ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Copyright © lookpolymers.com All Rights Reserved