Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA271009 Medium Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA271009 Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing NA 271-009 can only be made when the processing conditions, equipment and end use are known. For further suggestions, contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits. Film gauge: 1.25 mils.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D1505
Thickness 31.8 microns
1.25 mil
Melt Flow 1.2 g/10 min
1.2 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 400 %
400 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Dart Drop Test 60.0 g
0.132 lb
F<sub>50</sub>; ASTM D1709
Film Tensile Strength at Break, MD 24.8 MPa
3600 psi
ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
1% Secant Modulus, MD 331 MPa
48000 psi
ASTM D882
1% Secant Modulus, TD 379 MPa
55000 psi
ASTM D882
Optical Properties Metric English Comments
Haze 7.0 %
7.0 %
ASTM D1003
Gloss 90 %
90 %
at 60°; ASTM D2457