Polymer Property : Film Tensile Strength at Break, TD = 22.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, TD 22.1 - 44.8 MPa
3200 - 6500 psi
Average value: 30.3 MPa Grade Count:11
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil ESCOR™ AT 320 Cast Film Resin  (discontinued **)
ESCOR AT 320 provides excellent adhesion to a variety of substrates and other film components such as aluminum foil, polyolefins, polycarbonate, PET, etc.Information provided by ExxonMobil Chemical
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
LyondellBasell Petrothene® NA271009 Medium Density Polyethylene
ApplicationsPETROTHENE NA 271-009 is a medium density polyethylene resin designed to overwrap film applications. NA 271-009 exhibits good film optics and high stiffness. Regulatory StatusNA 271-009..
Film Tensile Strength at Break, TD 22.1 MPa
3210 psi
ASTM D882
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE
General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a..
Film Tensile Strength at Break, TD 22.1 MPa
3210 psi
D638
Westlake EF522 12% Ethylene Vinyl Acetate Copolymer
Westlake ELEVATE™ EF522 is an ethylene vinyl acetate copolymer with 12% VA. EF522 is designed for blown and cast films requiring excellent optics and low heat seal initiation. High melt strength m..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Westlake EN1817AA Low Density Polyethylene
Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Westlake EP310 Low Density Polyethylene
WESTLAKE polyethylene EP310 is a low-density polyethylene suggested for cast film bakery applications. This material has outstanding optical and processing properties.Application/UsesBakery bagsSoft..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin
Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation ..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LD 071.LQ Blown Film Resin
L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LD 071.LR Blown Film Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin
Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin
Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin
Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade)
Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin
Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: ..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Dow INTEGRAL™ 906 Multilayer Adhesive Film
INTEGRAL 906 Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethanes.Informa..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Dow INTEGRAL™ 909 Monolayer Adhesive Film / Automotive Headliners
INTEGRAL 909 Adhesive Film is a versatile heat-activated film that bonds to such substrates as: Polyethylene, Nylon, Polyester, Fiberglass, Polyurethane Foams, Wood, Paperboard, Cotton, Non-wovens,..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin
Resin Type: linear low density polyethylene, hexene copolymer, medium slip, cast/blown film resinCharacteristics: good optics, good drawdown, can be used straight or blended with LDPE or HDPE, can b..
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
ExxonMobil Escorene™ FL 00206 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: FL 00206 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 280°C (536°F) may cause resin degradation. Machines should always b..