Dow INTEGRAL™ 906 Multilayer Adhesive Film

Category Polymer , Film , Thermoset
Manufacturer Dow Chemical
Trade Name INTEGRAL™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow INTEGRAL™ 906 Multilayer Adhesive Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INTEGRAL 906 Adhesive Film is a heat-activated, thermally stable adhesive film capable of bonding to urethane foam-baked fabrics, polyester and nylon fabrics, fiberglass, and rigid urethanes.Information provided by Dow
Physical Properties Metric English Comments
Thickness 50.8 microns
2.00 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 480 %
480 %
ASTM D882
Film Elongation at Break, TD 520 %
520 %
ASTM D882
Secant Modulus, MD 0.0620 GPa
8.99 ksi
2% Secant; ASTM D882
Secant Modulus, TD 0.0690 GPa
10.0 ksi
2% Secant; ASTM D882
Elmendorf Tear Strength, MD 10.2 g/micron
260 g/mil
ASTM D882
Elmendorf Tear Strength, TD 14.2 g/micron
360 g/mil
ASTM D882
Film Tensile Strength at Break, MD 25.5 MPa
3700 psi
ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882