Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.59 GPa | 376 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Packaging M2288 Polyvinyl Chloride, Rigid (PVC, Rigid) Opaque sheet extrusion compound.Information provided by PolyOne |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | ASTM D638 |
PolyOne Nymax™ 600 A Natural F Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy HRA222 ASA (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material.This data was supplied by.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222 ASA+PC (Europe-Africa-Middle East) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant ASA+PC alloy for injection moulding processes. Typical properties as measured on natural material. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Tensile Modulus | 2.59 GPa @Temperature 23.0 °C |
376 ksi @Temperature 73.4 °F |
ASTM D638 |
PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC900 CPVC is an extrusion compound for CTS Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC900 demonstrates eas.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1432 PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in opaque colors. Typical minimum color tolerance limit is DE CMC < 1.0 |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KX06415 Acetal Copolymer LNP LUBRICOMP* KX06415 is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid Powder. Added features of this material include: Easy Molding, Heat Stabilized, Wear Resistant. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC LNP* STAT-KON* DX05301C is a compound based on Polycarbonate containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive, Low Ionic.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON DX11408 PC LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP (Asia Pacific) LNP* Thermocomp* MB006HS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22M Acetal Copolymer LNP LUBRICOMP* KAL22M is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare. |
|||
Tensile Modulus | 2.59 GPa | 376 ksi | ASTM Test |
BASF Ultraform H 2320 006 Q600 POM Ultraform H2320 006 is a high-molecular-weight grade of POM for injection molding. It conforms to FDA requirements of 21 CFR 177.2470. |
|||
Tensile Modulus | 2.59 GPa @Temperature 120 °C |
376 ksi @Temperature 248 °F |
ISO Data |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |