SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MB006HS PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MB006HS is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized, Healthcare.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm

@Time 86400 sec
0.010 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 23.4 %
23.4 %
ASTM D638
Tensile Modulus 2.59 GPa
376 ksi
50 mm/min; ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 2.04 GPa
296 ksi
ASTM D790
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.29 J/cm
4.29 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C

@Thickness 3.20 mm
145 °F

@Thickness 0.126 in
unannealed; ASTM D648