Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , Chlorinated PVC (CPVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Geon EC900 CPVC is an extrusion compound for CTS Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC900 demonstrates ease of processing and excellent thermal stability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Hardness, Shore D 84
84
ASTM D2240
Tensile Strength, Yield 49.0 MPa

@Temperature 23.0 °C
7110 psi

@Temperature 73.4 °F
ASTM D638
Tensile Modulus 2.59 GPa

@Temperature 23.0 °C
376 ksi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 91.7 MPa
13300 psi
ASTM D790
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 4.50 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
8.43 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Annealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Processing Properties Metric English Comments
Melt Temperature 198 - 210 °C
388 - 410 °F
Descriptive Properties Value Comments
Agency Ratings NSF 14
NSF 61
UL 94
Forms Powder
Generic Material CPVC
Generic Name Polyvinyl Chloride, Chlorinated (CPVC)
Processing Method Extrusion
Pipe Extrusion
PVC Cell Classification 24447
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Building Materials
Piping
Plumbing Parts
Users viewing this material also viewed the following: