Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.10 MPa
450 psi
ASTM D412
Polymax® Maxelast® F02-141J TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Strength, Yield 3.10 MPa
450 psi
@ 50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer
Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C)..
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer
With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band..
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer
Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r..
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer
Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d..
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 551 Perfluoroelastomer
With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz ..
Tensile Strength, Yield 3.10 MPa
450 psi
200%, post cured- 4 hours at 177°C; ASTM D412
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.10 MPa
450 psi
at 200%, post cured- 2 hours at 177°C; ASTM D412
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.10 MPa
450 psi
100%; ASTM D412
Teknor Apex APEX® 3311-55 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
Master Bond Mastersil 153 Two Component, High Temperature Resistance Silicone Adhesive
Master Bond MasterSil 153 is a two component, paste silicone compound for high performance bonding and sealing. MasterSil 153 is an addition cured system and does not require exposure to air for com..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
2 in/min; ASTM D638
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer
DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical ..
Tensile Strength, Yield 3.10 MPa
450 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer
Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited..
Tensile Strength, Yield 3.10 MPa
450 psi
50 mm/min cross speed, ASTM D638
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium
Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod..
Tensile Strength, Yield 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content
Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries.
Tensile Strength, Yield 3.10 MPa
450 psi
ASTM D638
Diamond Polymers Softflex® SF 6060 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Tensile Strength, Yield 3.10 MPa
450 psi
ACC MM922 Condensation Cure 2-Part Molding Rubber
Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing..
Tensile Strength, Yield 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
across flow; ASTM D412
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber  (discontinued **)
Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong..
Tensile Strength, Yield 3.10 MPa
450 psi
TM R050-36
Resinlab® SEC1233 Silver Filled Epoxy Adhesive
Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit..
Tensile Strength, Yield 3.10 - 21.0 MPa
450 - 3050 psi
Average value: 14.0 MPa Grade Count:25
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..