Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Diamond Polymers Softflex® SF 6060 Thermoplastic Elastomer Alloy

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Diamond and Network Polymers
Trade Name Softflex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Diamond Polymers Softflex® SF 6060 Thermoplastic Elastomer Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
ASTM D2240
Tensile Strength, Yield 3.10 MPa
450 psi
ASTM D638
Elongation at Yield 650 %
650 %
ASTM D638
Flexural Modulus 0.0344 GPa
4.99 ksi
ASTM D790
Izod Impact, Notched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Users viewing this material also viewed the following: