Greene Tweed CHEMRAZ® 550 Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer Greene Tweed
Trade Name CHEMRAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed CHEMRAZ® 550 Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in dynamic or static processing equipment applications with service temperatures up to 210°C (410°F).Applications:Valve sealsFitting and union sealsGasketsRegulator sealsFilter sealsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.93 g/cc
1.93 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ASTM D2240
Tensile Strength at Break 12.1 MPa
1750 psi
ASTM D1414
Tensile Strength, Yield 3.10 MPa
450 psi
@50% Elongation; ASTM D1414
7.93 MPa
1150 psi
@100% Elongation; ASTM D1414
Elongation at Break 140 %
140 %
ASTM D1414
Compression Set 25 %
25 %
70 hours @ 400°F (204°C) @ 25% deflection; ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Descriptive Properties Value Comments
Color Black