DuPont™ Surlyn® 8320 Ionomer Resin, Sodium

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer DuPont
Trade Name Surlyn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Surlyn® 8320 Ionomer Resin, Sodium.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sodium grade has low hardness and very low stiffness. Increased flexibility is achieved by incorporating a third co-monomer into the resin during polymerization. It is used alone or in combination with other ionomer resins or other polymers as a way to tailor flexibility for specific applications. In golf ball covers, for example, it provides a softer feel and imparts greater spin when the ball is in contact with the club face. Surlyn® 8320 is normally processed in a polymer blend by injection molding.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 36
36
ASTM D2240
Tensile Strength, Ultimate 18.6 MPa
2700 psi
ASTM D638
Tensile Strength, Yield 3.10 MPa
450 psi
50 mm/min cross speed, ASTM D638
Elongation at Break 555 %
555 %
ASTM D638
Flexural Modulus 0.0303 GPa
4.39 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Tensile Impact Strength 450 kJ/m²
214 ft-lb/in²
ASTM D1822S
Abrasion 61
61
NBS Index; ASTM D1630
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
DSC
Vicat Softening Point 47.0 °C
117 °F
Rate B, ASTM D1525-70