Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 3.10 MPa | 450 psi | ASTM D412 |
Polymax® Maxelast® F02-141J TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | @ 50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 505 Perfluoroelastomer Chemraz® 505, a perfluoroelastomer, provides a broader range of chemical resistance than any other compound on the market. With a temperature range of -22°F to 446°F (-30°C to 230°C).. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 555 Perfluoroelastomer With its broad chemical resistance, Chemraz® 555, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. Chemraz 555 provides a significantly wider operational band.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 565 Perfluoroelastomer Chemraz®, a proprietary Greene, Tweed compound, has the broadest chemical resistance of any elastomeric material. Chemraz combines the resilience and sealing force of an elastomer with chemical r.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 550 Perfluoroelastomer Chemraz ® 550 is recommended for use in wet systems where chemical compatibility is required and small amounts of contamination are acceptable. This seal material has a wide variety of uses in d.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 551 Perfluoroelastomer With its broad chemical resistance, Chemraz® 551 is ideally suited as a universal sealing material for aqueous semiconductor wafer processing and chemical/DI water distribution systems. Chemraz .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 200%, post cured- 4 hours at 177°C; ASTM D412 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | at 200%, post cured- 2 hours at 177°C; ASTM D412 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3311-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Automotive Applications, Food Service Applications, General Purpose, Medical Applications, Profiles, To.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | |
Master Bond Mastersil 153 Two Component, High Temperature Resistance Silicone Adhesive Master Bond MasterSil 153 is a two component, paste silicone compound for high performance bonding and sealing. MasterSil 153 is an addition cured system and does not require exposure to air for com.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 2 in/min; ASTM D638 |
A. Schulman SCHULAFLEX® SF 230 Ethylene-Based Butene Plastomer DescriptionSchulaflex SF230 is an ethylene-based butene plastomer. Available in natural as a non-UV stable product. It can be compounded as natural or colors with a full UV package.NOTE: Physical .. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® 8028N Thermoplastic Elastomer Elastocon® 8028N is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8028N is FDA compliant and well suited.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | 50 mm/min cross speed, ASTM D638 |
DuPont™ Surlyn® 8320 Ionomer Resin, Sodium Surlyn® 8320 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. This very low modulus sod.. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
|
Daikin DAI-EL G-902 Fluoroelastomer Terpolymer, Peroxide Curable Grade, 71% Fluorine Content Offers excellent chemical and steam resistance. Offers good mechanical characteristics.Features: Excellent solvent resistance, good mold flow.Information provided by Daikin Industries. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | ASTM D638 |
Diamond Polymers Softflex® SF 6060 Thermoplastic Elastomer Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | |
ACC MM922 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tensile Strength, Yield | 3.10 MPa @Strain 100 % |
450 psi @Strain 100 % |
across flow; ASTM D412 |
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Tensile Strength, Yield | 3.10 MPa | 450 psi | TM R050-36 |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |
|||
Tensile Strength, Yield | 3.10 - 21.0 MPa | 450 - 3050 psi | Average value: 14.0 MPa Grade Count:25 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |